Heptane, R0 =  0.691 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.890    4.610       6.021     1.695    1.1711      1.786         1
  1.000    2.390    5.440       8.984     1.784    1.2325      2.856         1
  1.000    3.190    6.580      14.504     1.941    1.3412      5.088         1
  1.000    5.010    9.110      31.538     2.222    1.5354     12.550         1
  1.000    5.530   10.120      38.671     2.205    1.5235     15.291         1

References:
1. R. F. Trunin , M. V. Zhernokletov, N. F. Kuznetsov, Yu. N. Sutulov, Shock
   compressibility of saturated and aromatic hydrocarbons, Khim. Fiz. 8(4),
   539-545 (1989) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g