Octyne, R0 =  0.760 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.900    4.700       6.787     1.679    1.2757      1.805         1
  1.000    2.340    5.260       9.354     1.801    1.3690      2.738         1
  1.000    3.150    6.190      14.819     2.036    1.5475      4.961         1
  1.000    4.140    7.520      23.661     2.225    1.6909      8.570         1
  1.000    4.810    8.610      31.475     2.266    1.7220     11.568         1
  1.000    5.480    9.240      38.483     2.457    1.8677     15.015         1

References:
1. R. F. Trunin, M. V. Zhernokletov, N. F. Kuznetsov, O. A. Radchenko, N. V.
   Sychevskaya, V. V. Shutov, Compression of liquid organic substances in shock
   waves, Khim. Fiz. 11(3), 424-432 (1992) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g