Dunite-2, R0 =  2.960 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.460    7.080      30.597     1.260    3.7290      1.066         1
  1.000    2.800    8.510      70.531     1.490    4.4115      3.920         1
  1.000    5.950   12.700     223.673     1.881    5.5692     17.701         1

References:
1. R. F. Trunin, V. I. Gonshakova, G. V. Simakov, N. E. Galdin, Investigation of
   rocks under high pressures and temperatures of shock compression, Izv. Akad.
   Nauk SSSR. Fiz. Zemli 9, 1-12 (1965) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g