Anhydrite, R0 =  2.970 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.730    4.860      10.537     1.177    3.4950      0.266         1
  1.000    1.180    5.680      19.906     1.262    3.7488      0.696         1
  1.000    1.550    6.290      28.956     1.327    3.9412      1.201         1
  1.000    1.850    6.610      36.319     1.389    4.1243      1.711         1
  1.000    2.420    7.430      53.402     1.483    4.4046      2.928         1
  1.000    2.770    7.990      65.733     1.531    4.5460      3.836         1
  1.000    3.240    8.790      84.585     1.584    4.7038      5.249         1
  1.000    3.710    9.650     106.331     1.625    4.8250      6.882         1
  1.000    1.550    6.290      28.956     1.327    3.9412      1.201         2

References:
1. G. V. Simakov, M. N. Pavlovskii, N. G. Kalashnikov, R. F. Trunin, Shock
   compressibility of twelve minerals, Izv. Akad. Nauk SSSR. Fiz. Zemli 8, 11-17
   (1974) [in Russian]
2. M. N. Pavlovskii, Measurements of sound velocity in quartzite, dolomite,
   anhydrite, sodiumn cloride, paraffin, plexiglas, polyethilene, and
   fluoroplast-4 under shock compression, Zh. Prikl. Mekh. Tekhn. Fiz. 5, 136-139
   (1976) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g