Beryl, R0 =  2.680 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.400    8.960      33.618     1.185    3.1763      0.980         1
  1.000    1.710    8.840      40.512     1.240    3.3227      1.462         1
  1.000    3.500    8.940      83.857     1.643    4.4043      6.125         1
  1.000    4.120    9.060     100.037     1.834    4.9151      8.487         1
  1.000    6.100   12.140     198.465     2.010    5.3866     18.605         1

References:
1. G. V. Simakov, R. F. Trunin, Minerals compression by shock waves, Izv. Akad.
   Nauk SSSR. Fiz. Zemli 2, 77-81 (1980) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g