Dolomite, R0 =  2.840 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.680    6.220      12.012     1.123    3.1886      0.231         1
  1.000    1.160    6.350      20.920     1.224    3.4748      0.673         1
  1.000    1.510    6.920      29.676     1.279    3.6327      1.140         1
  1.000    1.830    7.230      37.576     1.339    3.8024      1.674         1
  1.000    2.250    7.920      50.609     1.397    3.9670      2.531         1
  1.000    2.760    8.300      65.059     1.498    4.2549      3.809         1
  1.000    4.070   10.180     117.669     1.666    4.7318      8.282         1
  1.000    1.510    6.920      29.676     1.279    3.6327      1.140         2
  1.000    0.495    6.440       9.053     1.083    3.0765      0.123         3
  1.000    0.813    6.680      15.424     1.139    3.2335      0.330         3
  1.000    1.120    6.920      22.011     1.193    3.3884      0.627         3
  1.000    1.170    7.030      23.359     1.200    3.4070      0.684         3
  1.000    1.790    7.450      37.873     1.316    3.7382      1.602         3
  1.000    2.380    8.070      54.547     1.418    4.0279      2.832         3
  1.000    2.650    8.440      63.520     1.458    4.1398      3.511         3
  1.000    3.140    8.750      78.029     1.560    4.4296      4.930         3
  1.000    3.730    9.770     103.496     1.618    4.5938      6.956         3
  1.000    4.140   10.020     117.811     1.704    4.8396      8.570         3
  1.000    5.320   11.540     174.356     1.855    5.2691     14.151         3
  1.000    2.240    7.720      49.112     1.409    4.0009      2.509         4
  1.000    3.090    8.770      76.962     1.544    4.3850      4.774         4

References:
1. N. G. Kalashnikov, M. N. Pavlovskii, G. V. Simakov, R. F. Trunin, Dynamic
   compressibility of the minerals of calcite group, Izv. Akad. Nauk SSSR. Fiz.
   Zemli 2, 23-29 (1973) [in Russian]
2. M. N. Pavlovskii, Measurements of sound velocity in quartzite, dolomite,
   anhydrite, sodiumn cloride, paraffin, plexiglas, polyethilene, and
   fluoroplast-4 under shock compression, Zh. Prikl. Mekh. Tekhn. Fiz. 5, 136-139
   (1976) [in Russian]
3. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977), 427-429
4. R. F. Trunin, Shock compressibility of condensed matters in strong shock waves
   caused by underground nuclear explosions, Usp. Fiz. Nauk 164(11), 1215-1237
   (1994) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g