Hedenbergite, R0 =  3.420 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.100    5.880      22.121     1.230    4.2070      0.605         1
  1.000    1.410    6.740      32.502     1.265    4.3247      0.994         1
  1.000    2.420    7.210      59.673     1.505    5.1478      2.928         1
  1.000    2.740    7.750      72.624     1.547    5.2904      3.754         1
  1.000    3.620    9.160     113.405     1.653    5.6547      6.552         1

References:
1. G. V. Simakov, M. N. Pavlovskii, N. G. Kalashnikov, R. F. Trunin, Shock
   compressibility of twelve minerals, Izv. Akad. Nauk SSSR. Fiz. Zemli 8, 11-17
   (1974) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g