Microcline, R0 =  2.566 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.210    6.390      19.840     1.234    3.1654      0.732         1
  1.000    1.630    6.390      26.727     1.342    3.4447      1.328         1
  1.000    1.820    6.610      30.870     1.380    3.5410      1.656         1
  1.000    2.410    6.610      40.877     1.574    4.0384      2.904         1
  1.000    3.040    7.240      56.477     1.724    4.4233      4.621         1
  1.000    3.950    8.520      86.356     1.864    4.7839      7.801         1
  1.000    6.270   11.880     191.135     2.118    5.4339     19.656         1

References:
1. G. V. Simakov, M. N. Pavlovskii, N. G. Kalashnikov, R. F. Trunin, Shock
   compressibility of twelve minerals, Izv. Akad. Nauk SSSR. Fiz. Zemli 8, 11-17
   (1974) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g