Pyrite, R0 =  4.910 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.840    7.000      28.871     1.136    5.5795      0.353         1
  1.000    1.120    7.000      38.495     1.190    5.8452      0.627         1
  1.000    1.390    7.430      50.709     1.230    6.0400      0.966         1
  1.000    2.150    8.300      87.619     1.350    6.6265      2.311         1
  1.000    2.960    9.650     140.249     1.442    7.0824      4.381         1
  1.000    5.000   12.770     313.504     1.644    8.0696     12.500         1

References:
1. G. V. Simakov, M. N. Pavlovskii, N. G. Kalashnikov, R. F. Trunin, Shock
   compressibility of twelve minerals, Izv. Akad. Nauk SSSR. Fiz. Zemli 8, 11-17
   (1974) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g