Sfalerite, R0 =  3.950 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.630    5.020      12.492     1.144    4.5169      0.198         1
  1.000    1.110    5.000      21.923     1.285    5.0771      0.616         1
  1.000    1.520    4.940      29.660     1.444    5.7056      1.155         1
  1.000    2.410    6.060      57.688     1.660    6.5581      2.904         1
  1.000    2.700    6.360      67.830     1.738    6.8639      3.645         1
  1.000    3.560    8.100     113.902     1.784    7.0474      6.337         1

References:
1. G. V. Simakov, M. N. Pavlovskii, N. G. Kalashnikov, R. F. Trunin, Shock
   compressibility of twelve minerals, Izv. Akad. Nauk SSSR. Fiz. Zemli 8, 11-17
   (1974) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g