Neoprene, R0 =  1.439 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.136    4.366       7.137     1.352    1.9451      0.645         1
  1.000    1.532    5.013      11.051     1.440    2.0723      1.174         1
  1.000    2.079    5.725      17.127     1.570    2.2595      2.161         1
  1.000    2.091    5.758      17.326     1.570    2.2595      2.186         1
  1.000    2.097    5.744      17.333     1.575    2.2664      2.199         1
  1.000    1.136    4.366       7.137     1.352    1.9451      0.645         2
  1.000    1.532    5.013      11.051     1.440    2.0723      1.174         2
  1.000    2.079    5.725      17.127     1.570    2.2595      2.161         2
  1.000    2.091    5.758      17.326     1.570    2.2595      2.186         2
  1.000    2.097    5.744      17.333     1.575    2.2664      2.199         2

References:
1. R. G. McQueen, S. P. Marsh, J. W. Taylor, J. N. Fritz, W. J. Carter, The
   equation of state of solids from shock wave studies. - In: High Velocity
   Impact Phenomena / Ed. R.Kinslow. - New-York: Academic Press, p.293-417;
   appendies on pp. 515-568 (1970).
2. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g