Mononitrotoluene, R0 =  1.168 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.340    4.200       6.574     1.469    1.7152      0.898         1
  1.000    2.300    5.640      15.151     1.689    1.9723      2.645         1
  1.000    1.289    4.150       6.248     1.451    1.6942      0.831         2
  1.000    2.241    5.572      14.585     1.673    1.9538      2.511         2

References:
1. J. M. Walsh, M. H. Rice, Journal of Chemical Phisics. 26, 815 (1957)
2. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g