LX-04, R0 =  1.859 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.577    3.785       4.060     1.180    2.1934      0.166    1    1
  1.000    0.611    3.895       4.424     1.186    2.2049      0.187    1    1
  1.000    0.832    4.354       6.734     1.236    2.2982      0.346    1    1

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Remarks:
1. solvent-pressed, fine-grain HMX

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g