Cesium fluoride, R0 =  4.620 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.711    4.544      35.920     1.604    7.4103      1.464    1    1
  1.000    2.083    5.226      50.292     1.663    7.6819      2.169    1    1
  1.000    2.368    5.710      62.468     1.709    7.8935      2.804    1    1
  1.000    3.205    6.865     101.651     1.876    8.6657      5.136    1    1

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Remarks:
1. single-crystal

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g