Aluminum, 3033, R0 =  2.700 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.178    6.839      21.752     1.208    3.2618      0.694         1
  1.000    1.344    7.167      26.008     1.231    3.3232      0.903         1
  1.000    1.491    7.382      29.718     1.253    3.3834      1.112         1

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g