Gold-germanium(9.3) alloy, R0 = 15.536 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.000    2.934       0.000     1.000   15.5360      0.000         1
  1.000    0.304    3.229      15.250     1.104   17.1507      0.046         1
  1.000    0.643    3.450      34.464     1.229   19.0948      0.207         1
  1.000    0.939    4.054      59.141     1.301   20.2192      0.441         1
  1.000    1.344    4.813     100.497     1.387   21.5551      0.903         1
  1.000    1.669    5.344     138.568     1.454   22.5917      1.393         1
  1.000    1.670    5.341     138.573     1.455   22.6036      1.394         1
  1.000    1.857    5.731     165.341     1.479   22.9832      1.724         1
  1.000    2.159    6.149     206.251     1.541   23.9426      2.331         1

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g