Iron-silicon(6.9) alloy, R0 =  7.490 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.975    5.706      41.670     1.206    9.0336      0.475         1
  1.000    1.092    5.850      47.848     1.230    9.2090      0.596         1
  1.000    2.291    7.929     136.058     1.406   10.5336      2.624         1

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g