Gabro, Bytowhite, Duluth, Minnesota, R0 =  2.919 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.877    5.965      15.270     1.172    3.4221      0.385         1
  1.000    0.878    5.954      15.259     1.173    3.4239      0.385         1
  1.000    0.886    5.717      14.786     1.183    3.4543      0.393         1
  1.000    0.910    5.286      14.041     1.208    3.5260      0.414         1
  1.000    1.187    5.688      19.708     1.264    3.6888      0.704         1
  1.000    1.677    5.569      27.261     1.431    4.1768      1.406         1
  1.000    2.314    6.432      43.445     1.562    4.5593      2.677         1
  1.000    2.314    6.472      43.716     1.557    4.5435      2.677         1
  1.000    2.314    6.640      44.850     1.535    4.4804      2.677         1
  1.000    2.660    6.847      53.164     1.635    4.7734      3.538         1
  1.000    3.017    7.124      62.738     1.735    5.0633      4.551         1
  1.000    3.058    7.509      67.028     1.687    4.9245      4.676         1
  1.000    3.059    7.786      69.523     1.647    4.8080      4.679         1
  1.000    3.059    7.983      71.282     1.621    4.7324      4.679         1

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g