Gabro, San Marcos, Escondido, California, R0 =  2.978 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.864    5.825      14.988     1.174    3.4966      0.373         1
  1.000    0.870    5.706      14.784     1.180    3.5137      0.378         1
  1.000    0.875    5.721      14.908     1.181    3.5157      0.383         1
  1.000    0.877    5.711      14.916     1.181    3.5183      0.385         1
  1.000    1.153    5.912      20.300     1.242    3.6995      0.665         1
  1.000    1.212    5.849      21.111     1.261    3.7564      0.734         1
  1.000    1.629    5.783      28.054     1.392    4.1458      1.327         1
  1.000    1.692    5.918      29.820     1.400    4.1703      1.431         1
  1.000    2.294    6.432      43.941     1.554    4.6289      2.631         1
  1.000    2.294    6.541      44.685     1.540    4.5866      2.631         1
  1.000    2.294    6.630      45.293     1.529    4.5535      2.631         1
  1.000    2.597    6.892      53.302     1.605    4.7787      3.372         1
  1.000    3.019    7.776      69.911     1.635    4.8680      4.557         1
  1.000    3.020    7.815      70.285     1.630    4.8536      4.560         1

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g