Sulfur, rhombic, R0 =  2.050 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.015    0.897    4.176       7.567     1.255    2.5726      0.402         1
  1.015    1.431    4.503      13.017     1.444    2.9610      1.024         1
  1.015    1.470    4.520      13.422     1.460    2.9936      1.080         1
  1.015    1.952    5.254      20.717     1.568    3.2141      1.905         1
  1.015    1.964    5.036      19.979     1.615    3.3114      1.929         1
  1.015    1.964    5.162      20.479     1.591    3.2606      1.929         1
  1.015    2.046    5.153      21.297     1.634    3.3502      2.093         1
  1.057    1.220    4.200       9.941     1.334    2.7342      0.744         2
  1.057    1.540    4.540      13.564     1.432    2.9359      1.186         2
  1.057    2.220    5.090      21.922     1.678    3.4406      2.464         2
  1.057    2.710    5.580      29.336     1.840    3.7718      3.672         2
  1.057    3.360    6.910      45.042     1.842    3.7762      5.645         2
  1.057    4.000    7.940      61.615     1.907    3.9095      8.000         2
  1.057    4.460    8.640      74.757     1.956    4.0100      9.946         2

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)
2. R. F. Trunin, L.F.Gudarenko, M. V. Zhernokletov, G. V. Simakov, Experimental
   data on shock compressibility and adiabatic expansion of condensed substances,
   RFNC, Sarov (2001) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g