Periclase-quartz(50) mixture, R0 =  1.577 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.825    3.455       9.944     2.120    3.3427      1.665         1
  1.000    2.399    4.375      16.552     2.214    3.4916      2.878         1
  1.000    2.748    4.811      20.849     2.332    3.6776      3.776         1
  1.000    3.515    5.608      31.086     2.679    4.2254      6.178         1
  1.000    3.523    6.164      34.246     2.334    3.6807      6.206         1
  1.000    3.868    6.675      40.717     2.378    3.7501      7.481         1

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g