Paraffin(16)-Tungsten(84) mixture, R0 =  4.510 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.590    4.330      31.050     1.580    7.1271      1.264         1
  1.000    1.620    4.260      31.125     1.614    7.2775      1.312         1
  1.000    2.590    5.620      65.647     1.855    8.3651      3.354         1
  1.000    2.950    6.120      81.424     1.931    8.7070      4.351         1
  1.000    5.370    9.040     218.937     2.463   11.1091     14.418         1

References:
1. Yu. F. Alekseev, L. V. Al'tshuler, V. P. Krupnikova, Shock compression of
   two-component paraffin-tungsten mixes, Zh. Prikl. Mekh. Tekhn. Fiz. 4, 152-155
   (1971) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g