Gabro, Russia, R0 =  2.890 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.780    5.740      12.939     1.157    3.3445      0.304         1
  1.000    1.180    5.850      19.950     1.253    3.6202      0.696         1
  1.000    1.440    5.810      24.179     1.330    3.8423      1.037         1
  1.000    1.560    5.940      26.780     1.356    3.9193      1.217         1
  1.000    2.140    6.470      40.014     1.494    4.3183      2.290         1
  1.000    2.600    7.210      54.176     1.564    4.5199      3.380         1
  1.000    3.070    7.730      68.583     1.659    4.7939      4.712         1
  1.000    3.630    8.280      86.863     1.781    5.1461      6.588         1
  1.000    3.840    8.890      98.658     1.760    5.0875      7.373         1

References:
1. R. F. Trunin, G. V. Simakov, I. P. Dudoladov, G. S. Telegin, I. P. Trusov,
   Rocks compressibility in shock waves, Izv. Akad. Nauk SSSR. Fiz. Zemli 1,
   52-58 (1988) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g