Copper chloride, R0 =  4.160 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.250    3.150       3.276     1.086    4.5186      0.031         1
  1.000    0.370    3.160       4.864     1.133    4.7117      0.068         1
  1.000    0.700    3.240       9.435     1.276    5.3065      0.245         1
  1.000    1.020    3.240      13.748     1.459    6.0714      0.520         1
  1.000    1.270    3.610      19.072     1.543    6.4178      0.806         1
  1.000    1.540    4.130      26.459     1.595    6.6335      1.186         1
  1.000    2.130    4.920      43.595     1.763    7.3359      2.268         1
  1.000    2.750    5.650      64.636     1.948    8.1048      3.781         1

References:
1. G. V. Simakov, I. I. Maksimov, S. S. Batsanov, Shock compressibilities of CuCl
   and TiI, Fiz. Goreniya i Vzriva. 31(4), 77-78 (1995) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g