PBX 9405-01, RDX-3 wt% NC-3 wt% CEF, R0 =  1.761 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.394    3.152       2.187     1.143    2.0126      0.078         1
  1.000    0.404    3.195       2.273     1.145    2.0159      0.082         1
  1.000    0.488    3.400       2.922     1.168    2.0561      0.119         1
  1.000    0.496    3.225       2.817     1.182    2.0811      0.123         1
  1.000    0.567    3.594       3.589     1.187    2.0909      0.161         1
  1.000    0.730    3.841       4.938     1.235    2.1742      0.266         1
  1.000    0.932    4.152       6.815     1.289    2.2707      0.434         1

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g