TATB - 10 wt% Kel F 800, reprocessed TATB, R0 =  1.912 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.074    4.728       9.709     1.294    2.4740      0.577         1
  1.000    1.239    4.905      11.620     1.338    2.5582      0.768         1
  1.000    1.449    4.982      13.803     1.410    2.6962      1.050         1
  1.000    1.522    5.259      15.304     1.407    2.6907      1.158         1

References:
1. S. P. Marsh (Ed.), LASL Shock Hugoniot Data, (Univ. California Press,
   Berkeley, 1980)

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g