Rubidium bromide, R0 =  3.290 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.080    3.160      11.228     1.519    4.9983      0.583    1    1
  1.000    1.380    3.620      16.436     1.616    5.3169      0.952    1    1
  1.000    1.730    4.160      23.678     1.712    5.6323      1.496    1    1
  1.000    1.960    4.440      28.631     1.790    5.8902      1.921    1    1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977), 477-482

Remarks:
1. Pressed

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g