Chlorine trifluoride - Aluminum, R0 =  2.061 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.120    3.550       8.195     1.461    3.0109      0.627         1
  1.000    1.530    4.320      13.622     1.548    3.1912      1.170         1
  1.000    2.070    5.200      22.185     1.661    3.4240      2.142         1
  1.000    2.950    6.440      39.155     1.845    3.8031      4.351         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977), 610-611

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g