RDX-TNT-Al-WAX, HBX-1, R0 =  1.750 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.000    2.860       0.000     1.000    1.7500      0.000         1
  1.000    0.580    3.810       3.867     1.180    2.0642      0.168         1
  1.000    0.835    4.347       6.352     1.238    2.1661      0.349         1
  1.000    0.855    4.368       6.536     1.243    2.1759      0.366         1
  1.000    0.977    4.707       8.048     1.262    2.2084      0.477         1
  1.000    1.000    4.767       8.342     1.265    2.2146      0.500         1
  1.000    1.020    4.550       8.122     1.289    2.2557      0.520         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977), 614-629

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g