RDX-TNT-Al-WAX, HBX-6, R0 =  1.760 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.000    2.760       0.000     1.000    1.7600      0.000         1
  1.000    0.000    2.820       0.000     1.000    1.7600      0.000         1
  1.000    0.560    3.970       3.913     1.164    2.0490      0.157         1
  1.000    0.985    4.450       7.715     1.284    2.2603      0.485         1
  1.000    1.005    4.482       7.928     1.289    2.2687      0.505         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977), 614-629

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g