Magnesium-lithium alloy, R0 =  1.463 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.570    5.320       4.437     1.120    1.6386      0.162         1
  1.000    0.900    5.800       7.637     1.184    1.7317      0.405         1
  1.000    1.960    6.790      19.470     1.406    2.0567      1.921         1
  1.000    2.590    7.540      28.570     1.523    2.2285      3.354         1
  1.000    2.800    7.830      32.075     1.557    2.2774      3.920         1
  1.000    3.420    8.450      42.279     1.680    2.4577      5.848         1
  1.000    4.590    9.850      66.145     1.873    2.7396     10.534         1

References:
1. R. F. Trunin, M. Yu. Belyakova, M. V. Zhernokletov, Yu. N. Sutulov, Shock
   compression of metallic alloys, Izv. Akad. Nauk SSSR. Fiz. Zemli 2, 99-106
   (1991) [in Russian] (Bull. Acad. Sci. USSR, Physics of the Solid Earth (1991))

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g