Lutetium, R0 =  9.740 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.540    2.760      14.517     1.243   12.1092      0.146         1
  1.000    1.170    3.380      38.518     1.529   14.8965      0.684         1
  1.000    2.160    4.530      95.304     1.911   18.6170      2.333         1
  1.000    4.600    8.560     383.522     2.162   21.0541     10.580         1

References:
1. L. V. Al'tshuler, A. A. Bakanova, I. P. Dudoladov, Effect of electrons
   structure on the shock compressibility of metals at high pressure, Zh. Eksp.
   Teor. Fiz. 53, 1967-1976 (1967) [in Russian] (Sov. Phys. - JETP 26(6),
   1115-1120 (1968))

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g