Brass, alloy 1163, R0 =  8.480 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.520    5.950      76.693     1.343   11.3896      1.155         1
  1.000    1.580    6.120      81.998     1.348   11.4312      1.248         1
  1.000    1.730    6.320      92.717     1.377   11.6762      1.496         1
  1.000    2.070    6.650     116.732     1.452   12.3127      2.142         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977), 640-649

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g