Magnesium-bismuth alloy, R0 =  2.440 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    1.000    4.540      11.078     1.282    3.1293      0.500         1
  1.000    1.320    4.860      15.653     1.373    3.3498      0.871         1
  1.000    1.540    6.050      22.734     1.341    3.2732      1.186         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977), 682-688

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g