Epoxy armstrong C-7 - Activator A, R0 =  1.198 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.600    3.700       2.660     1.194    1.4299      0.180         1
  1.000    0.780    4.070       3.803     1.237    1.4820      0.304         1
  1.000    1.180    4.690       6.630     1.336    1.6007      0.696         1
  1.000    1.520    5.330       9.706     1.399    1.6759      1.155         1
  1.000    1.830    5.820      12.760     1.459    1.7475      1.674         1
  1.000    1.900    5.730      13.043     1.496    1.7923      1.805         1
  1.000    2.360    6.480      18.321     1.573    1.8842      2.785         1
  1.000    2.380    6.480      18.476     1.580    1.8934      2.832         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977), 741-746

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g