Niobium(70)-tantalum(30) alloy, R0 =  9.930 g/cc

    m        U        D           P        R/R0      R         E-E0    Rem  Ref
  1.000    0.900    5.250      46.919     1.207   11.9845      0.405         1
  1.000    1.710    6.350     107.825     1.369   13.5895      1.462         1
  1.000    2.320    7.050     162.415     1.490   14.8005      2.691         1
  1.000    4.320    9.920     425.544     1.771   17.5903      9.331         1

References:
1. A. A. Bakanova, I. P. Dudoladov, Yu. N. Sutulov, Fulfillment of additive law
   for shock-compressed alloys, Zh. Prikl. Mekh. Tekhn. Fiz. 6, 167-172 (1972)
   [in Russian] (J. Appl. Mech. Techn. Phys. 13 (1972))

Denotions:
R0   - normal density of substance, g/cc
R00  - initial density of sample, g/cc
P0   - initial gas pressure (for gaseous substances only), GPa
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g