Polymethylmethacrylate (Plexiglas), R0 =  1.186 g/cc

    m        U0       P0       U        P     Rem  Ref
  1.005    4.080   40.634    4.370   37.430         1
  1.005    4.080   40.634    4.670   24.835         1
  1.005    4.080   40.634    5.160   20.675         1
  1.005    4.080   40.634    5.640   14.497         1
  1.005    4.080   40.634    7.600    1.935         1
  1.005    4.080   40.634    8.140    1.518         1
  1.005    4.080   40.634    8.190    0.841         1
  1.005    4.080   40.634    9.270    0.170         1

References:
1. A. V. Bushman, M. V. Zhernokletov, I. V. Lomonosov, Yu. N. Sutulov, V. E.
   Fortov, K. V. Khishchenko, Investigation of plexiglas and teflon under double
   shock waves loading and isentropic expansion. Plastics equation of state at
   high energy density, Dokl. Akad. Nauk SSSR 329(5), 581-584 (1993) [in Russian]

Denotions:
R0 - normal density of substance, g/cc
m  - porosity of sample
U0 - particle velocity on shock Hugoniot, km/s
P0 - pressure on shock Hugoniot, GPa
U  - particle velocity, km/s
P  - pressure, GPa