Polymethylmethacrylate (Plexiglas), R0 =  1.186 g/cc

    m        U        D        Cs          P        R/R0      R          E-E0   Rem  Ref
  1.005    1.660    5.290    6.570      10.362     1.450    1.7196      1.378         1
  1.005    2.130    5.880    7.560      14.779     1.560    1.8502      2.268         1

References:
1. M. N. Pavlovskii, Measurements of sound velocity in quartzite, dolomite,
   anhydrite, sodiumn cloride, paraffin, plexiglas, polyethilene, and
   fluoroplast-4 under shock compression, Zh. Prikl. Mekh. Tekhn. Fiz. 5, 136-139
   (1976) [in Russian]

Denotions:
R0   - normal density of substance, g/cc
m    - porosity of sample
U    - particle velocity, km/s
D    - shock wave velocity, km/s
Cs   - sound velocity, km/s
P    - pressure behind shock front, GPa
R/R0 - compression ratio behind shock front
R    - density behind shock front, g/cc
E-E0 - specific energy behind shock front, kJ/g