Iron , R0 =  7.800 g/cc

Target: 
  Sample density R0 = 7.8 g/cc, bulk sound velocity C0 = 4.65 km/s, longitudial sound velocity Cl = 5.97 km/s
  Sample thickness 12 mm (rod)
Loading: 
  High explosive in contact with sample
Experiment type: Capacitor gauge

     t, mks     V, m/s

      0.000      0.000
      0.100     35.000
      0.300     43.000
      0.400     61.000
      0.500    200.000
      0.590    500.000
      0.700    535.000
      0.800    535.000
      1.000    527.000
      1.500    500.000
      2.150    456.000
      2.400    482.000
      2.500    487.000
      2.750    493.000
      3.000    491.000
      3.200    482.000

References:
1. G. I. Kanel', A. A. Razorenov, A. V. Utkin, K. Baumung, Experimental profiles
   of shock waves, Preprint of Scientific Association IVTAN of RAS (1996)