Lead, R0 = 11.346 g/cc

Target: 
  Sample density R0 = 11.35 g/cc, bulk sound velocity C0 = 2.03 km/s, longitudial sound velocity Cl = 2.25 km/s
  Sample thickness 3.75 mm (cast and pressed)
  Aluminum baseplate 4 mm thick
Loading: 
  Aluminum impactor 1.9 mm thick, impactor velocity 2000 +/- 70 m/s
Experiment type: Laser interferometer (VISAR)

     t, mks     V, m/s

      0.048      0.000
      0.048    198.000
      0.048   1201.000
      0.050   1354.500
      0.054   1354.530
      0.075   1350.000
      0.171   1309.390
      0.236   1307.550
      0.311   1309.000
      0.536   1308.080
      0.750   1307.220
      0.964   1307.680

References:
1. G. I. Kanel', A. A. Razorenov, A. V. Utkin, K. Baumung, Experimental profiles
   of shock waves, Preprint of Scientific Association IVTAN of RAS (1996)