Polystyrene, R0 =  1.050 g/cc

    m        U1       P1      dU12      P2    Rem  Ref
  1.000    4.580   40.700    0.840   67.200         1
  1.000    4.580   40.700    1.400   83.100         1
  1.000    4.580   40.700    2.510  130.100         1

References:
1. A. V. Bushman, M. V. Zhernokletov, I. V. Lomonosov, Yu. N. Sutulov, V. E.
   Fortov, K. V. Khishchenko, Experimental investigation of fenilon and
   polystyrene under shock loading and isentropic expansion. Equations of state
   of plastics at high energy densities), Zh. Eksp. Teor. Fiz. 109(5), 1662-1670
   (1996) [in Russian] (JETP 82(5), 895-899 (1996))

Denotions:
R0    - normal density of substance, g/cc
m     - porosity of sample
U1    - particle velocity on shock Hugoniot, km/s
P1    - pressure on shock Hugoniot, GPa
dU12  - jump of particle velocity on the front of reflected shock wave, km/s
P2    - pressure behind the second shock, GPa