Lithium hydride, R0 =  0.742 g/cc

    m        U1       P1      dU12      P2    Rem  Ref
  0.991    0.005    0.037   -2.205   13.740         1
  0.991    0.005    0.038   -1.655    9.630         1
  0.991    0.007    0.047   -0.813    3.630         1
  0.991    0.008    0.051   -1.132    5.540         1
  0.991    0.010    0.066   -0.860    3.840         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977), 434-437

Denotions:
R0    - normal density of substance, g/cc
m     - porosity of sample
U1    - particle velocity on shock Hugoniot, km/s
P1    - pressure on shock Hugoniot, GPa
dU12  - jump of particle velocity on the front of reflected shock wave, km/s
P2    - pressure behind the second shock, GPa