Steel, 1055 alloy, R0 =  7.825 g/cc

    m        U1       P1      dU12      P2    Rem  Ref
  1.000    0.028    1.450   -0.197    9.210         1
  1.000    0.031    1.450   -0.316   14.050         1
  1.000    0.031    1.450   -0.200    9.450         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977), 182-191

Denotions:
R0    - normal density of substance, g/cc
m     - porosity of sample
U1    - particle velocity on shock Hugoniot, km/s
P1    - pressure on shock Hugoniot, GPa
dU12  - jump of particle velocity on the front of reflected shock wave, km/s
P2    - pressure behind the second shock, GPa