Aluminium oxide, ceramic, R0 =  3.980 g/cc

    m        U1       P1      dU12      P2    Rem  Ref
  1.000    0.228    9.900   -0.732   36.600         1
  1.000    0.253   11.100   -0.707   36.900         1
  1.000    0.262   11.400   -0.233   18.500         1
  1.000    0.284   12.300   -0.211   19.600         1
  1.000    0.368   16.100   -0.109   19.900         1
  1.044    0.200    7.900   -0.670   26.300         1
  1.044    0.260   10.000   -0.030   10.700         1
  1.045    0.210    8.400   -0.100   11.300         1
  1.045    0.220    8.500   -1.060   43.200         1
  1.045    0.180    6.700   -0.670   25.900         1
  1.045    0.210    8.100   -1.050   42.400         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977)

Denotions:
R0    - normal density of substance, g/cc
m     - porosity of sample
U1    - particle velocity on shock Hugoniot, km/s
P1    - pressure on shock Hugoniot, GPa
dU12  - jump of particle velocity on the front of reflected shock wave, km/s
P2    - pressure behind the second shock, GPa