Magnesium oxide, single cristal, R0 =  3.676 g/cc

    m        U1       P1      dU12      P2    Rem  Ref
  1.000    0.105    3.450   -0.530   16.600         1
  1.000    0.121    3.990   -0.504   16.800         1
  1.000    0.248    8.900   -1.102   42.300         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977)

Denotions:
R0    - normal density of substance, g/cc
m     - porosity of sample
U1    - particle velocity on shock Hugoniot, km/s
P1    - pressure on shock Hugoniot, GPa
dU12  - jump of particle velocity on the front of reflected shock wave, km/s
P2    - pressure behind the second shock, GPa