Forsterite polycristalline, R0 =  3.119 g/cc

    m        U1       P1      dU12      P2    Rem  Ref
  1.184    0.031    0.480   -0.979   11.300         1
  1.185    0.031    0.470   -1.179   15.900         1
  1.187    0.031    0.470   -0.999   11.600         1

References:
1. M. van Thiel (Ed.), Compendium of shock wave data, (Livermore: Lawrence
   Livermore Laboratory Report UCRL-50108, 1977)

Denotions:
R0    - normal density of substance, g/cc
m     - porosity of sample
U1    - particle velocity on shock Hugoniot, km/s
P1    - pressure on shock Hugoniot, GPa
dU12  - jump of particle velocity on the front of reflected shock wave, km/s
P2    - pressure behind the second shock, GPa